MATERIAL OPTIONS
​
​
​
​
​
​
​
​
ONYX FULL DENSITY
Tensile Modulus (GPa) 2.4
Tensile Stress at Yield (MPa) 40
Tensile Stress @ Break (MPa) 37
Tensile Strain at Break (%) 25
Flexural Strength (MPa) 71
Flexural Modulus (GPa) 3.0
Heat Deflection Temp (C) 145
Density 1.2
Onyx Flexural Strength: 71 MPa
Onyx is a micro carbon fiber filled nylon.
It’s 1.4 times stronger and stiffer than ABS and can be reinforced with any continuous fiber.
Onyx sets the bar for surface finish, chemical resistivity, and heat tolerance.
​
​
​
​
​
​
​
​
​
​
​
​
ALUMINUM ALLOY 333
Tensile Strength (MPa) 193 [28000 psi]
Tensile Modulus (GPa) 73 [10600 ksi]
Shear Strength (F) 119 (MPa) [17300 psi]
Hardness (F) Range 65-100 HB
Tensile Strength (T6) Min 241 MPa [35000 psi]
Shear Strength (T6) 147 (MPa) [21300 psi]
Hardness (T6) Range 85-115 HB
Density 2.77 [173 lb/ft])
​